New 3D FUN website for purchases in the EU. We are still working on the website. If you are interested in goods from the 3dfun.cz website, please write to info@3dfun.cz and we will solve it.
You cannot fill out this field

Jamghe 10K Resin 1 L - Engineering like

Code: 1560/TMA
Brand: Jamghe
37,08 € / pcs 30,64 € excl. VAT
Category: Resins
Color: Tmavě šedá (Nebula gray) 10K Engineering
In stock (10 pcs) | 1560/TMA
37,08 € / pcs
30,64 € excl. VAT
Color: Šedá (Grey) 10K Engineering
In stock (9 pcs) | 2355/SED
37,08 € / pcs
30,64 € excl. VAT
Color: Bílá (White) 10K Engineering
In stock (5 pcs) | 2355/BIL
37,08 € / pcs
30,64 € excl. VAT
Color: Černá (Black) 10K Engineering
In stock (5 pcs) | 2355/CER
37,08 € / pcs
30,64 € excl. VAT
Color: Transparentní světle modrá (Transparent light blue) 10K Engineering
Sold out | 2355/TRA
37,08 € / pcs
30,64 € excl. VAT
Color: Transparentní tmavě modrá (Transparent dark blue) 10K Engineering
In stock (2 pcs) | 2355/TRA2
37,08 € / pcs
30,64 € excl. VAT

Resin

Material Properties:

  • UV resin or synthetic resin.
  • It works byusing laser/light radiation (UV), which hardens the liquid resin in layers.
  • The most precise printing method, known for its details and smooth surface.
  • Suitable for use on SLA, DLP and LCD printers.

Technical Parameters:

  • Hardness: 80-88 D (according to Shore test)
  • Viscosity: 300-550 mPa.s
  • Density: 1.05-1.25 g/cmᶟ
  • Volume: 1 L
  • Flexural strength: +/- 44.15 MPa
  • Tensile strength: +/- 38.36 MPa
  • Curing wavelength: 405 nm

Printing parameters recommended by the manufacturer (per layer 0.05 mm):

  • First layers: 35-45 s
  • Other layers: 2-5 s

+ Does not become brittle or crack.

+ Good workability, can be drilled, impacted, etc. into prints...

+ Suitable for printing machine parts from gears to clips.

+ Scratch resistant.

+ Weather resistant.

+ Highly strong and tough.

+ Has 90% of ABS properties.

- Risk of allergic reaction or adverse health problems. We recommend working with a respirator and rubber gloves, preferably in a well-ventilated room.

- Before starting printing (preferably 30 mins), shake and then let it stand to eliminate bubbles.

- After printing, it needs to be washed (e.g., in isopropyl alcohol) and cured under UV light with a wavelength of 405 nm.